MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Versalis EDISTIR PD RK6223N High Impact Polystyrene (HIPS)  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Symbol according to ISO 1043-1: S/B
Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23

Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI 415/94. It exhibits easy flow and is particularly recommended for injection molding of telectronic equipments.

Applications: Developed for TV back covers, monitor and printer housings.

Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains release agent. Contains release agent.

ISO data. Information provided by Enichem

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 200 °C
cm³/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPa50 mm/min
Elongation at Break 35 %Nominal
Elongation at Yield 1.5 %50 mm/min
Tensile Modulus 2.20 GPa1 mm/min
Charpy Impact Unnotched 7.50 J/cm²
 6.50 J/cm²
@Temperature -30.0 °C
Charpy Impact, Notched 0.800 J/cm²
 0.450 J/cm²
@Temperature -30.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
Dielectric Constant 2.5
@Frequency 100 Hz
Dielectric Strength 65.0 kV/mm
Dissipation Factor 0.00040
@Frequency 100 Hz
Comparative Tracking Index 500 V
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 81.0 °C50°C/hr; 50N
Flammability, UL94 HB
@Thickness 1.50 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Americas Styrenics EA6740 High Impact Polystyrene
Chevron Phillips EC6600 HIPS - High Impact Polystyrene
Americas Styrenics EB6400 High Impact Polystyrene
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene
Videolar-Innova 825 E High Impact Polystyrene (HIPS)

PENI62 / 35869

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.