- Grade designed specially for extrusion and thermoforming
- Characteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusion
Features: - Stress crack resistance
- Good temperature resistance
Applications: - Refrigerator and packaging
- Sheet, film and profile extrusion
Information provided by Dax Resinas |