MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion BrushCAST® 165CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Pouring Temperature: 1010-1120°C
Heat treatment required for max strength (Annealing): 760-790°C/water quench
Heat treatment required for max strength (Hardening): 760-790°C/water quench

Description: The unique combination of physical and mechanical properties of copper beryllium casting alloys provide a dynamic range of metallurgical alternatives to meet specific performance requirements. The inherent strength, hardness, conductivity, and castability of these materials make them ideal for applications which require a high performance engineered material solution. Advancements in component casting technology and proprietary material production technology pioneered by Brush Wellman have resulted in BrushCAST™ alloys being a cost effective design choice.

BrushCAST™ high strength casting alloys are available in fine grain equivalents. Material properties and manufacturing characteristics are similar to those of the standard casting alloys. Grain refinement is achieved through precise additions of either cobalt or titanium. Fine grain casting alloys are preferred in applications where excellent surface finish characteristics are required in the cast product.

Information supplied by Brush Wellman Engineered Materials.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: UNS C82400
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.304 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 34 - 39
Tensile Strength, Ultimate 145000 - 155000 psi
Tensile Strength, Yield 135000 - 145000 psi
@Strain 0.2 %
Elongation at Break 2 - 4 %
Modulus of Elasticity 19000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000688 - 0.00000860 ohm-cmConductivity is 20-25% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 21.1 - 204 °C
Thermal Conductivity 696 BTU-in/hr-ft²-°F
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 1.6 - 1.85 %
Cobalt, Co 0.20 - 0.65 %
Copper, Cu 98 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IBC Advanced Alloys Thermal Mould™ Super Mold and Die Copper Alloy, Beryllium-Free
Commercial Rolled Zinc (Zn-0.06Pb-0.06Cd), Cold-Rolled - Longitudinal Properties
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO15 Temper wire
CMW® ELKONITE® TC53 Heat Treatable Tungsten Carbide Copper material
CMW® 73 Copper Alloy

NBBC30 / 15340

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.