MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

IBC Advanced Alloys Thermal Mould™ Super Mold and Die Copper Alloy, Beryllium-Free
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Thermal Mould™ Super is manufactured to provide a combination of high strength and hardness properties coupled with superior thermal properties. This range of properties makes Thermal-Mould™ Super the premier material for copper alloy molds and a wide range of other applications from oil and gas to aerospace.

Information provided by IBC Advanced Alloys.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.69 g/cc0.314 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 26 - 3026 - 30Heat Treated plate and round bars
Tensile Strength 758 - 862 MPa110000 - 125000 psiHeat Treated plate and round bars
Tensile Strength, Yield 621 - 724 MPa
@Strain 0.2 %
90000 - 105000 psi
@Strain 0.2 %
Heat Treated plate and round bars
Elongation at Break 5.0 - 7.0 %5.0 - 7.0 %Heat Treated plate and round bars
Modulus of Elasticity 128 GPa18500 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.5 µm/m-°C9.70 µin/in-°F
Thermal Conductivity 156 W/m-K1080 BTU-in/hr-ft²-°F
Melting Point 982 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 1.0 %1.0 %
Copper, Cu 91 %91 %As Balance
Nickel, Ni 7.0 %7.0 %
Silicon, Si 2.0 %2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ECOMold 95 Copper Mold Material
CMW® 73 Copper Alloy
Cadi MOLD-MOR™ 40
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17300)
Materion BrushCAST® 165CT Fine Grain Casting Alloy (Solution Annealed & Aged)

NIBCA940 / 177694

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.