MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
FloMet Fe-50% Ni Soft Magnetic Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume metal powder and 40% volume plastic. The mixture (referred to as feedstock) is then injection molded at relatively low temperatures and pressures in conventional plastic injection molding machines. The molded green parts are then thermally processed in two steps. First, the binder is removed by evaporation in an operation called debinding. Next, the part is sintered in a dry hydrogen atmosphere, which densifies the part isotropically. The complex shape of the original molded part is retained throughout the process, and close tolerances can be achieved. Density is typically 95-98% of the wrought metal; mechanical properties and corrosion resistance are similar to wrought material

Information provided by FloMet LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 45
Tensile Strength, Ultimate 60000 psi
Tensile Strength, Yield 20000 psi
@Strain 0.2 %
Elongation at Break 25 %
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability <= 55000µmax in G/Oe with a magnetizing field of 25 Oe.
Magnetic Coercive Force, Hc 0.11 Oe
Magnetic Saturation Flux Density, Bmax 14400 GaussMagnetizing field of 25 Oe.
 15200 GaussMagnetizing field of 500 Oe.
Magnetic Remanence, Br 9100 GaussMagnetizing field of 25 Oe.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.050 %
Iron, Fe 50 %As remainder
Nickel, Ni 50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
FloMet Fe-50%Co Soft Magnetic Alloy
ATI Allegheny Ludlum AL 4750™ Electrical Alloy, UNS K94800 or UNS K95000
FloMet Fe-3% Si Soft Magnetic Alloy
FloMet Fe-42% Ni Controlled Expansion Alloy
FloMet Permalloy® 4-79 Moly Soft Magnetic Alloy

NXFLOM09 / 20020

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.