MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low-to-high levels of conductivity depending upon application requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 119 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 10300 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 159 MPaASTM D790
Flexural Modulus 8270 MPaASTM D790
Izod Impact, Notched 53.0 J/m
@Thickness 6.35 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1000 ohm - 1e+05ASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
Flammability, UL94 V-1
@Thickness 3.00 mm
BKUL Listed; UL 94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 266 - 282 °C
Middle Barrel Temperature 271 - 288 °C
Front Barrel Temperature 277 - 293 °C
Mold Temperature 71.1 - 116 °C
 
Descriptive Properties
FeaturesElectromagnetic Shielding (EMI)
 ESD Protection
 Flame Retardant
 Radio Frequency Shielding (RFI)
Filler / ReinforcementNickel-Coated Carbon Fiber
FormsPellets
Generic MaterialABS+PC
Generic NameAcrylonitrile Butadiene Styrene + PC (ABS+PC)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAerospace Applications
 Business Equipment
 Electrical Parts
 Electrical/Electronic Applications
 Housings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber
Covestro Bayblend® FR630 GR PC/ABS Blend
Techmer ES Plastiblend® PC/ABS FR 6206 UV
Avient Edgetek® CY-1000 UV FR V0 Acrylonitrile Butadiene Styrene + PC (ABS+PC)

PH0POL1272 / 145841

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.