MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper, UNS C19700, H06 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent soldering and brazing. Excellent capacity for both cold and hot forming.

Applications: Electrical and electronic connectors, circuit breaker components, fuse clips, cable shielding, and lead frames. Generally suited to applications requiring excellent formability combined with high strength and conductivity.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7373
Tensile Strength, Ultimate 480 MPa69600 psi
Tensile Strength, Yield 470 MPa68200 psiStrip
Elongation at Break 3.0 %3.0 %In 50 mm
Modulus of Elasticity 121 GPa17500 ksi
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000216 ohm-cm
@Temperature 20.0 °C
0.00000216 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.8 µm/m-°C
@Temperature 20.0 - 100 °C
9.89 µin/in-°F
@Temperature 68.0 - 212 °F
 18.8 µm/m-°C
@Temperature 20.0 - 200 °C
10.4 µin/in-°F
@Temperature 68.0 - 392 °F
 19.3 µm/m-°C
@Temperature 20.0 - 300 °C
10.7 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 320 W/m-K2220 BTU-in/hr-ft²-°F
Melting Point 1069 - 1086 °C1956 - 1987 °F
Solidus 1069 °C1956 °F
Liquidus 1086 °C1987 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 450 - 600 °C842 - 1110 °F
Hot-Working Temperature 750 - 950 °C1380 - 1740 °F
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co <= 0.050 %<= 0.050 %
Copper, Cu 99.15 %99.15 %
Iron, Fe 0.30 - 1.2 %0.30 - 1.2 %
Lead, Pb <= 0.050 %<= 0.050 %
Magnesium, Mg 0.010 - 0.20 %0.010 - 0.20 %
Manganese, Mn <= 0.050 %<= 0.050 %
Phosphorus, P 0.10 - 0.40 %0.10 - 0.40 %
Tin, Sn <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
High Strength Modified Copper, UNS C19400, O50 Temper flat products
MetalTek C18100 Chrome Zirc Copper High Conductivity
Johnson Matthey Pallabraze™ 1090 Palladium Based Brazing Alloy
High Strength Modified Copper, UNS C19400, O82 Temper flat products
High Strength Modified Copper, UNS C19400, O60 Temper flat products

MC19700b3 / 10976

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.