MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

CLAL-MSX NICLAL 1800 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Main Characteristics:
  • Good corrosion resistance
  • High mechanical properties
Typical Applications:
  • Parts subject to high stress
  • High quality fasteners

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 155 - 185155 - 185
Tensile Strength, Ultimate 480 - 650 MPa69600 - 94300 psi
Tensile Strength, Yield >= 450 MPa
@Strain 0.2 %
>= 65300 psi
@Strain 0.2 %
Elongation at Break >= 10 %>= 10 %100 A
Modulus of Elasticity 130 GPa18900 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000260 ohm-cm0.0000260 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C
@Temperature 0.000 - 100 °C
8.89 µin/in-°F
@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 30.0 W/m-K208 BTU-in/hr-ft²-°F
Melting Point 1060 °C1940 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 62 %62 %
Lead, Pb <= 1.0 %<= 1.0 %
Nickel, Ni 18 %18 %
Zinc, Zn <= 19 %<= 19 %
 
Descriptive Properties
ColorSilvery

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Techical Ceramics MYCROSINT® CD Boron Nitride
3M Techical Ceramics MYCROSINT® SO 20 Boron Nitride
3M Techical Ceramics MYCROSINT® S Boron Nitride
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Rolled Copper Alloy
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Drawn Copper Alloy

NCLAL087 / 160118

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.