MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.41 - 1.87 g/cc0.0509 - 0.0676 lb/in³Average value: 1.67 g/cc Grade Count:59
Filler Content 10.0 - 50.0 %10.0 - 50.0 %Average value: 28.9 % Grade Count:22
Water Absorption 0.0200 - 0.0500 %0.0200 - 0.0500 %Average value: 0.0243 % Grade Count:14
Water Absorption at Saturation 0.0200 - 0.0300 %0.0200 - 0.0300 %Average value: 0.0275 % Grade Count:4
Additive Loading 10.0 - 30.0 %10.0 - 30.0 %Average value: 25.7 % Grade Count:7
Viscosity  220000 - 220000 cP
@Temperature 310 - 310 °C
220000 - 220000 cP
@Temperature 590 - 590 °F
Average value: 220000 cP Grade Count:1
 220000 - 220000 cP
@Frequency 100 - 100 Hz
220000 - 220000 cP
@Frequency 100 - 100 Hz
Average value: 220000 cP Grade Count:1
Linear Mold Shrinkage 0.000500 - 0.00800 cm/cm0.000500 - 0.00800 in/inAverage value: 0.00257 cm/cm Grade Count:52
Linear Mold Shrinkage, Transverse 0.00400 - 0.00850 cm/cm0.00400 - 0.00850 in/inAverage value: 0.00650 cm/cm Grade Count:12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 117 - 121117 - 121Average value: 120 Grade Count:6
Tensile Strength, Ultimate 26.2 - 180 MPa3800 - 26100 psiAverage value: 128 MPa Grade Count:55
Tensile Strength, Yield 131 - 159 MPa19000 - 23000 psiAverage value: 141 MPa Grade Count:5
Elongation at Break 0.800 - 3.00 %0.800 - 3.00 %Average value: 1.71 % Grade Count:57
Modulus of Elasticity 5.86 - 20.0 GPa850 - 2900 ksiAverage value: 11.9 GPa Grade Count:45
Flexural Yield Strength 45.5 - 250 MPa6600 - 36300 psiAverage value: 184 MPa Grade Count:54
Flexural Modulus 4.90 - 17.9 GPa710 - 2600 ksiAverage value: 10.9 GPa Grade Count:54
Flexural Strain at Break 1.40 - 3.00 %1.40 - 3.00 %Average value: 2.14 % Grade Count:5
Compressive Yield Strength 62.1 - 96.5 MPa9000 - 14000 psiAverage value: 83.7 MPa Grade Count:3
Izod Impact, Notched 0.320 - 0.854 J/cm0.600 - 1.60 ft-lb/inAverage value: 0.686 J/cm Grade Count:42
Izod Impact, Unnotched 1.07 - 6.94 J/cm2.00 - 13.0 ft-lb/inAverage value: 3.98 J/cm Grade Count:36
Izod Impact, Notched (ISO) 6.40 - 9.80 kJ/m²3.05 - 4.66 ft-lb/in²Average value: 8.53 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 20.0 - 40.0 kJ/m²9.52 - 19.0 ft-lb/in²Average value: 32.0 kJ/m² Grade Count:5
Charpy Impact Unnotched 1.80 - 4.50 J/cm²8.57 - 21.4 ft-lb/in²Average value: 3.42 J/cm² Grade Count:12
Charpy Impact, Notched 0.600 - 1.20 J/cm²2.86 - 5.71 ft-lb/in²Average value: 0.879 J/cm² Grade Count:12
Falling Dart Impact 2.60 - 7.20 J1.92 - 5.31 ft-lbAverage value: 4.40 J Grade Count:3
Instrumented Impact Total Energy 1.97 - 3.07 J1.45 - 2.26 ft-lbAverage value: 2.50 J Grade Count:3
Coefficient of Friction 0.140 - 0.4400.140 - 0.440Average value: 0.261 Grade Count:9
Coefficient of Friction, Static 0.110 - 0.3800.110 - 0.380Average value: 0.257 Grade Count:8
K (wear) Factor 8.50 - 141 x 10-8 mm³/N-M4.22 - 70.0 x 10-10 in³-min/ft-lb-hrAverage value: 65.2 x 10-8 mm³/N-M Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.00e+17 ohm-cm1.00e+12 - 1.00e+17 ohm-cmAverage value: 1.06e+16 ohm-cm Grade Count:18
Surface Resistance 1.00e+12 - 1.00e+15 ohm1.00e+12 - 1.00e+15 ohmAverage value: 3.34e+14 ohm Grade Count:3
Dielectric Constant 3.40 - 4.203.40 - 4.20Average value: 3.91 Grade Count:8
Dielectric Strength 13.8 - 26.0 kV/mm350 - 660 kV/inAverage value: 18.5 kV/mm Grade Count:9
Dissipation Factor 0.00100 - 0.004000.00100 - 0.00400Average value: 0.00189 Grade Count:8
Comparative Tracking Index 125 - 250 V125 - 250 VAverage value: 167 V Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.8 - 32.4 µm/m-°C6.00 - 18.0 µin/in-°FAverage value: 21.5 µm/m-°C Grade Count:10
 15.0 - 15.0 µm/m-°C
@Temperature 100 - 200 °C
8.33 - 8.33 µin/in-°F
@Temperature 212 - 392 °F
Average value: 15.0 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 35.0 - 45.0 µm/m-°C19.4 - 25.0 µin/in-°FAverage value: 40.0 µm/m-°C Grade Count:3
 110 - 110 µm/m-°C
@Temperature 100 - 200 °C
61.1 - 61.1 µin/in-°F
@Temperature 212 - 392 °F
Average value: 110 µm/m-°C Grade Count:1
Thermal Conductivity 0.303 - 0.400 W/m-K2.10 - 2.78 BTU-in/hr-ft²-°FAverage value: 0.368 W/m-K Grade Count:3
Melting Point 278 - 284 °C532 - 543 °FAverage value: 280 °C Grade Count:9
Maximum Service Temperature, Air 220 - 260 °C428 - 500 °FAverage value: 235 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 260 - 280 °C500 - 536 °FAverage value: 266 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 232 - 277 °C450 - 531 °FAverage value: 259 °C Grade Count:53
Vicat Softening Point 240 - 260 °C464 - 500 °FAverage value: 253 °C Grade Count:4
Flammability, UL94 HB - V-0HB - V-0Grade Count:43
 
Processing PropertiesMetricEnglishComments
Processing Temperature 288 - 370 °C550 - 698 °FAverage value: 309 °C Grade Count:7
Nozzle Temperature 320 - 350 °C608 - 662 °FAverage value: 332 °C Grade Count:3
Melt Temperature 282 - 370 °C540 - 698 °FAverage value: 318 °C Grade Count:44
Mold Temperature 51.7 - 200 °C125 - 392 °FAverage value: 151 °C Grade Count:50
Drying Temperature 50.0 - 150 °C122 - 302 °FAverage value: 138 °C Grade Count:42
Moisture Content 0.0200 - 0.0500 %0.0200 - 0.0500 %Average value: 0.0395 % Grade Count:22
Injection Pressure 4.96 - 124 MPa720 - 18000 psiAverage value: 81.6 MPa Grade Count:33

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

O4553 / 78355

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.