MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Bales Mold Service Hard Chrome QQ-C-320 Mold Coating
Categories: Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Description: Hard Chrome provides excellent wear resistance to glass filled resins. It can be selectively plated up to .020 for shims and inside or outside diameter corrections that need E.D.M. or grinding to finished size. Hard Chrome is a great way to save precision pieces that cannot be welded.

Information provided by Bales Mold Service Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 7272
Coefficient of Friction <= 0.20<= 0.20
 
Processing PropertiesMetricEnglishComments
Processing Temperature 54.4 °C130 °FApplied Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chromium Nitride (CrN) PVD Coating
Aluminum Titanium Nitride (AlTiN) PVD Coating
Titanium Carbonitride (TiCN) PVD Coating
Titanium Nitride (TiN) Coating
XADC-Armoloy Armoloy® TDC Hard Chromium Coating

NBAL1 / 15080

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.