MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chromium Nitride (CrN) PVD Coating
Categories: Ceramic; Nitride; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This silver/gray coating offers excellent corrosion resistance, while its enhanced thermal stability and oxidation resistance improves performance in cutting and forming of copper, nickel, Monel, and titanium metals and alloys. Offers improved performance with die casting of aluminum and zinc, replacement of hard chrome plating, copper machining, and glass fabrication.. As with TiN, feeds and speeds can be increased and tool life can improve by as much as 800%. Forming operations with abrasive materials should see improvements beyond those experienced with TiN. Typical coating thickness is 1-5 µm. Adhesion measured by scratch test is 100.0 N.

Data provided by BryCoat Inc.

Key Words: Hard Ceramic Coatings; Brycoat; Mold Coating; Aerospace Coatings
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.90 g/cc0.213 lb/in³
Thickness 0.250 - 15.0 microns0.00984 - 0.591 mil
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 2000 - 25002000 - 2500typical
Hardness, Rockwell C >= 80>= 80
Vickers Microhardness 2000 - 25002000 - 2500typical
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.200.20
Shear Modulus 83 GPa12000 ksicalculated
Coefficient of Friction 0.40.4steel vs. coating; typical
 0.05 - 0.90.05 - 0.9range of published values
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 0.000300 ohm-cm>= 0.000300 ohm-cmliterature values for single crystal are higher.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 700 °C1290 °FOxidation Begins
Heat of Formation 125 kJ/mol125 kJ/mol
Decomposition Temperature 1050 °C1920 °F
 1500 °C2730 °F
 
Descriptive Properties
ColorSilver Gray
Crystal StructureCubic
Scratch Adhesion Value> 3.0 kgfhard steel substrates

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chromium Nitride
Titanium Nitride (TiN) Coating
Titanium Aluminum Nitride (TiAlN) PVD Coating
Aluminum Titanium Nitride (AlTiN) PVD Coating
Titanium Carbonitride (TiCN) PVD Coating

BNTiCR / 273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.