MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Adflex Q 200 F Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adflex Q 200 F is a reactor TPO (thermoplastic polyolefin) manufactured using Lyondell Basell's proprietary Catalloy process technology. Adflex Q 200 F features a fractional melt flow and a low modulus. It is selected by customers for use in extrusion applications. This resin is ideal for making soft hygienic or heavy duty films. It can also be used to modify LDPE or LLDPE resins in order to improve puncture resistance and other mechanical characteristics to allow further down gauging. It contains no slip or antiblock. This grade is available in natural pellet form.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; North America; South & Central America

Application: Cured in Place Pipe; Interior Automotive Applications; Soft Profile & Sheets; Specialty Film; TPO Foils and Skins

Market: Automotive; Flexible Packaging

Processing Method: Blown Film; Calendaring; Extrusion Blow Molding; Sheet and Profile Extrusion

Attribute: Good Flexibility; Good Impact Resistance; Good Processability; Good Toughness; High Strength; Low Flow

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccMethod A; ISO 1183-1
Melt Flow 0.800 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35.0
@Time 15.0 sec
ISO 868
Tensile Strength at Break 13.0 MPaISO 527-1, -2
Tensile Strength, Yield 8.00 MPaISO 527-1, -2
Elongation at Break 500 %ISO 527-1, -2
Elongation at Yield 18.0 %ISO 527-1, -2
Flexural Modulus 150 MPaISO 178
Charpy Impact, Notched 2.10 kJ/m²
@Temperature -40.0 °C
Complete Break; ISO 179
 60.0 kJ/m²
@Temperature 23.0 °C
Partial Break; ISO 179
 87.0 kJ/m²
@Temperature -20.0 °C
Partial Break; ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °CUnannealed; ISO 75B-1, -2
Vicat Softening Point 76.0 °CA/50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 44.0 %
@Thickness 1.14 mm
ASTM D1003
Gloss 86.0 %
@Thickness 1.14 mm
60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9007 / 323935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.