Adflex Q 200 F is a reactor TPO (thermoplastic polyolefin) manufactured using Lyondell Basell's proprietary Catalloy process technology. Adflex Q 200 F features a fractional melt flow and a low modulus. It is selected by customers for use in extrusion applications. This resin is ideal for making soft hygienic or heavy duty films. It can also be used to modify LDPE or LLDPE resins in order to improve puncture resistance and other mechanical characteristics to allow further down gauging. It contains no slip or antiblock. This grade is available in natural pellet form. Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; North America; South & Central America Application: Cured in Place Pipe; Interior Automotive Applications; Soft Profile & Sheets; Specialty Film; TPO Foils and Skins Market: Automotive; Flexible Packaging Processing Method: Blown Film; Calendaring; Extrusion Blow Molding; Sheet and Profile Extrusion Attribute: Good Flexibility; Good Impact Resistance; Good Processability; Good Toughness; High Strength; Low Flow Information provided by LyondellBasell. |