MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Adstif EA 5075 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Adstif is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability.

Adstif EA5075 is a high flow heterophasic copolymer with low TVOC, good process ability, good stiffness and impact balance.   Typical customer applications are components of compound for automotive and electrical appliances.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D 792
Melt Flow 60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
60 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 30.0 MPa4350 psiASTM D 638
Elongation at Yield 5.0 %5.0 %ASTM D 638
Flexural Modulus 1.60 GPa232 ksiASTM D 790
Izod Impact, Notched  0.200 J/cm
@Temperature -20.0 °C
0.375 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.500 J/cm
@Temperature 23.0 °C
0.937 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FASTM D648
Vicat Softening Point 150 °C302 °FASTM D1525
 
Descriptive Properties
Processing MethodCompounding, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Adstif EA5076 Polypropylene Copolymer
PolyMirae Adstif EA5075 Polypropylene Copolymer
LyondellBasell Adstif HA 899J Polypropylene
LyondellBasell Adstif HA 5029 Polypropylene
LyondellBasell Adstif HA 1152 Polypropylene

PEQT7032 / 218671

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.