MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Adstif HA 1152 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Adstif is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability.

Adstif HA1152 is a high crystalline homopolymer designed for injection molding applications with high process ability. It features extremely high stiffness, high flowability, high gloss. Adstif HA1152 has been especially developed for the production of stiff injection molded articles, where high rigidity is needed. Typical applications of Adstif HA1152 would include packaging containers, house wares, appliances, technical parts.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 93.0 MPa13500 psiISO 2039-1
Tensile Strength, Yield 40.0 MPa5800 psiISO 527-1,-2
Elongation at Break 15 %15 %ISO 527-1,-2
Elongation at Yield 6.0 %6.0 %ISO 527-1,-2
Tensile Modulus 2.00 GPa290 ksiISO 527-1,-2
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 104 °C219 °FB50; ISO 306
 158 °C316 °FA50; ISO 306
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Adstif HA 748L Polypropylene
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
ExxonMobil PP1074KNE1 Polypropylene Homopolymer
LyondellBasell Hostacom PP HU42L 205199 Polypropylene
ExxonMobil Exceed™ PP7905E1 Polypropylene Homopolymer

PEQT7028 / 218667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.