MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Master Bond UV10TKLO-2 UV Curable Compound for Aerospace Applications
Categories: Polymer; Adhesive

Material Notes: Description: Master Bond UV10TKLO-2 is a special one component UV curable epoxy modified system for high performance bonding, sealing and encapsulation. This system has passed rigorous testing to meet low outgassing specifications, as per NASA ASTM E-595. UV10TKLO-2 has high clarity and cures readily at room temperature when exposed to UV light. The ideal wavelengths for curing are 320-365 nm and the desired energy is 20-40 milliwatts per cm². The UV system is not inhibited by oxygen. UV10TKLO-2 offers resistance to water as well as to various acids, bases and solvents. The epoxy features superior physical strength properties and its service temperature range is from -60°F to +300°F. UV10TKLO-2 can be cured in thicker sections, up to 1/16 of an inch and can be easily “layered” to higher levels. Most significantly, the low outgassing properties enable this UV to be used in a wide array of optical, electro-optical and vacuum applications that until now have been “off limits” for UV curable epoxies. It should be noted that to optimize the outgassing properties, UV10TKLO-2 should be preheated to approximately 50°C for 15 minutes prior to use and then allowed to cool down to room temperature. UV10TKLO-2 is a first class electrical insulator.

Product Advantages:

  • One component: no mixing required.
  • Exceptionally fast curing with UV light source.
  • Not oxygen inhibited.
  • High viscosity with excellent clarity and light transmission.
  • Excellent physical strength, electrical insulation and chemical resistance profile.
  • Meets NASA low outgassing test, ASTM E-595, specifications.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Water Absorption <= 1.0 %<= 1.0 %1 week immersion
Viscosity  10000 - 20000 cP
@Temperature 40.0 °C
10000 - 20000 cP
@Temperature 104 °F
 225000 - 275000 cP
@Temperature 25.0 °C
225000 - 275000 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 8580 - 85
Tensile Strength at Break >= 41.4 MPa>= 6000 psi
Tensile Modulus >= 1.38 GPa>= 200 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.6
@Frequency 60 Hz,
Temperature 25.0 °C
3.6
@Frequency 60 Hz,
Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original unopened container

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 760 Hybrid Adhesive Sealant
Aptek UVIBOND 7100 Semi-rigid, UV-Curing Urethane Adhesive
Master Bond UV22 One Component, UV Curable, Nanosilica Reinforced Epoxy System
Henkel Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive

PMASTB364 / 149611

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.