MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aptek UVIBOND 7100 Semi-rigid, UV-Curing Urethane Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: UVIBOND 7100 is an unfilled, one component, electrically insulating, transparent, semi-rigid urethane adhesive designed for bonding polycarbonate, ABS, glass and other various substrates. UVIBOND 7100 is fully curable when exposed to the proper UV radiation.

U.V. curable for extremely fast production output; Semi-rigid for high strength bonds with a degree of flexibility; Low viscosity for easy handling and substrate wetting; Low ionic impurities for electrical/electronic applications; Thixotropic version available for doming and staking applications designated as APTEK 97034

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D1475
Viscosity 4000 cP4000 cPASTM D1824
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595Property taken 1 hr after U.V. exposure, 1/16" casting; ASTM D2240
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 760 Hybrid Adhesive Sealant
Master Bond UV10TKLO-2 UV Curable Compound for Aerospace Applications
Henkel Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive
Master Bond UV24TKLO One Component, UV-Curable, Low Outgassing Adhesive System
Master Bond UV22 One Component, UV Curable, Nanosilica Reinforced Epoxy System

PAPTEK10 / 24172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.