MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TechnylStar™ AFX 218S V50 PA6, 50% glass filled, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Description: High stiffness materials TECHNYLSTAR Polyamide 66, reinforced with 50% of glass fiber, heat stabilized for injection molding. Characterized by a high fluidity of the melt.

Available in: Asia Pacific

Product Applications: TECHNYLSTAR AFX 218S V50 BLACK 31N is used in automotive industry and industrial parts, demanding high mechanical strength, stiffness, thermal stability and excellent surface aspect, by a very easy flow and low injection molding pressure. This grade is widely used for automotive parts such as structural parts, brackets and pulleys. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccISO 1183/A
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0034 cm/cm
Linear Mold Shrinkage, Transverse 0.0042 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ASTM D786
Tensile Strength, Yield 230 MPaASTM D638
Elongation at Break 2.5 %ASTM D638
Flexural Strength 355 MPaASTM D790
Flexural Modulus 16000 MPaASTM D790
Izod Impact, Notched 180 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 256 °CASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
1210
 
Processing PropertiesOriginal ValueComments
Feed Temperature 260 - 270 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned
Domo Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Domo TechnylStar™ AFX 218 V50 PA6, 50% glass filled
Domo TechnylStar™ SX 216 V50 PA6, 50% glass filled, DRY
Domo TechnylStar™ SX 216 V50 PA6, 50% glass filled, Conditioned

PRHOD823 / 138054

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.