MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestodur® X7190 Heat Stabilized PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Description: VESTODUR X7190 and X7390 are unreinforced, heat-stabilized and polymer modified polybutylene terephthalate (PBT) compounds with low shrinkage for extrusion. The compounds are especially suitable for the manufacture of stiff, small diameter tubing, e.g., loose buffering for fiber optics. VESTODUR X7390 has increased hydrolysis and heat resistance. Compared with standard PBT compounds X7190 and X7390 are harder. Therefore, they can also be used to protect as outer sheaths to protect electrical cables from the chewing of rodents. Both compounds contain a processing aid which facilitates feeding in the extrusion process.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccISO 1183
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
@Thickness 2.00 mm
sheet with film gate at rim, mold temperature 80°C
Linear Mold Shrinkage, Transverse 0.012 - 0.014 cm/cm
Melt Flow 10.24 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87ISO 868
Tensile Strength, Yield 61.0 MPaISO 527-1/2
Elongation at Break >= 50 %ISO 527-1/2
Elongation at Yield 6.5 %ISO 527-1/2
Tensile Modulus 2.40 GPaISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 0.650 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
Longitudinal; ISO 11359, DIN 53752
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359, DIN 53752
Vicat Softening Point 150 °CMethod B, 50 N; ISO 306
 210 °CMethod A, 10 N; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
IEC 60695
 HB
@Thickness 1.60 mm
IEC 60695

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestodur® 1003 PBT
Eurotec® Tecodur® PB70 NL PBT, unfilled, natural
Barlog Plastics KEBATER B511T PBT unreinforced, super tough
Barlog Plastics KEBATER B510 PBT unreinforced
A. Schulman COMTUF® 420 Impact Modified PBT

PHUMA64 / 47578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.