MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay N1000 Nylon Mesh
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Flow media. Ideally suited to infusion applications.

Features & Benefits:

  • Open nylon 6 mesh suitable for resin infusion processing up to 204°C (400°F). The open mesh allows for easy flow of resin to ensure complete substrate saturation during the infusion process
  • Compatible with most commonly used infusion resins, with the exception of phenolic systems
  • The nylon 6 construction allows for easy removal when the infusion process is complete

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 508 micronsat the intersection
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66)
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (Cond)
Solvay VI5
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
Solvay Vac-Pak® A6200 Fluoropolymer Film

PCYTED240 / 180542

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.