MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Property data for molded test bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/ccASTM D792
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Filler Content 33 %33 %Glass Fiber Reinforcement
Water Absorption 0.90 %0.90 %24h/23C; ISO 62
 1.0 %1.0 %@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 136 MPa19700 psiISO 527
Tensile Strength, Yield 169 MPa24500 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 8.8 %8.8 %ISO 527
Elongation at Yield 3.0 %3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 1.82 GPa264 ksiISO 527
 8.62 GPa1250 ksiASTM D638
 8.78 GPa1270 ksiISO 178
Flexural Strength 172 MPa24900 psiASTM D790
 207 MPa30000 psiISO 178
Flexural Modulus 8.62 GPa1250 ksiASTM D790
Izod Impact, Notched 0.910 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.70 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 227 °C441 °FAnnealed; ISO 75-2/A
 221 °C
@Thickness 3.18 mm
430 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 271 - 293 °C520 - 559 °F
Mold Temperature 82.2 - 107 °C180 - 225 °F
Drying Temperature 82.2 °C180 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
AdditiveUV Stabilizer
AppearanceBlack
FeaturesGeneral Purpose
 Good UV Resistance
 Heat Stabilized
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (Cond)
Solvay N1000 Nylon Mesh
RheTech Products G10P100-00 10% Glass Fiber Reinforced Polypropylene, Natural
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer

PH0POL1079 / 145648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.