MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 50H1 PA66, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This phosphorus and halogen free flame retardant grade, offers excellent filling qualities combined with good stiffness. It is particularly suitable for molding insulating parts for electrical components: Components for electrical connections: junction blocks, terminal blocks, and connectors. This product is available in natural. Other colors can be provided upon request

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 46.0 MPaISO 527 Type 1A
Tensile Strength, Yield 53.0 MPaISO 527 type 1 A
Tensile Modulus 2200 MPaISO 527 Type 1A
Flexural Strength 61.0 MPaISO 178
Flexural Modulus 1710 MPaISO 178
Charpy Impact Unnotched NBISO 179/1eU
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 50H1 PA66, DRY
Kolon KOPA® KN333G15 G/F Reinforced Nylon 66
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Conditioned)
Kolon KOPA® KN133G30 G/F Reinforced Nylon 6
Kolon KOPA® KN3321G15VO G/F Reinforced & Flame Retardant Nylon 66

PRHOD716 / 137947

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.