MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 50H1 PA66, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This phosphorus and halogen free flame retardant grade, offers excellent filling qualities combined with good stiffness. It is particularly suitable for molding insulating parts for electrical components: Components for electrical connections: junction blocks, terminal blocks, and connectors. This product is available in natural. Other colors can be provided upon request

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183/A
Water Absorption 0.88 %
@Temperature 23.0 °C,
Time 86400 sec
0.88 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 78.0 MPa11300 psiISO 527 Type 1A
Tensile Strength, Yield 86.0 MPa12500 psiISO 527 type 1 A
Elongation at Break 10 %10 %ISO 527 Type 1A
Elongation at Yield 4.2 %4.2 %ISO 527 type 1 A
Tensile Modulus 3.80 GPa551 ksiISO 527 Type 1A
Flexural Strength 137 MPa19900 psiISO 178
Flexural Modulus 3.70 GPa537 ksiISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 8.00 J/cm²38.1 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.320 J/cm²1.52 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 237 °C459 °FISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FISO 75/Af
Flammability, UL94  V-0
@Thickness 0.380 mm
V-0
@Thickness 0.0150 in
1210
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
1210
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
1210
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
1210
Glow Wire Ignition Temperature 725 °C
@Thickness 1.60 mm
1340 °F
@Thickness 0.0630 in
ISO 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 260 - 270 °C500 - 518 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone265-275°C
Mixing Zone265-275°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 50H1 PA66, Conditioned
Envalior Akulon® K225-KS PA6 FR(30), Dry, Flame Retardant, Heat Stabilized
Covestro Apec® 1895 Polycarbonate
EMS-Grivory Grivory® XE 4185 black 9453 PA*
Domo Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH50

PRHOD715 / 137946

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.