MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ceradyne CeraTrex™ SC-P2 Silicon Carbide  (discontinued **)
Categories: Ceramic; Carbide

Material Notes:

Features:

  • purity>99.9995%
  • corrosion resistance
  • wear resistance
  • near net shape fabrication to 400 mm OD
  • Applications:

  • semiconductor components
  • wear components
  • Information provided by Ceradyne Company

    Ceradyne was acquired by 3M in 2012. The product line has been extensively renamed and reconfigured.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 3.20 g/cc0.116 lb/in³
    Weibull Modulus 1212
     
    Mechanical PropertiesMetricEnglishComments
    Vickers Microhardness 285028500.3 kg/mm²
    Modulus of Elasticity 440 GPa63800 ksi
    Flexural Strength 375 MPa
    @Temperature 23.0 °C
    54400 psi
    @Temperature 73.4 °F
    Poissons Ratio 0.170.17
    Fracture Toughness 3.10 MPa-m½2.82 ksi-in½
    Shear Modulus 188 GPa27300 ksicalculated
    Abrasion 11781178Abrasive Wear Resistance Parameter
     
    Electrical PropertiesMetricEnglishComments
    Electrical Resistivity 10.0 ohm-cm10.0 ohm-cm
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear 4.50 µm/m-°C
    @Temperature 20.0 - 1000 °C
    2.50 µin/in-°F
    @Temperature 68.0 - 1830 °F
    Thermal Conductivity 200 W/m-K1390 BTU-in/hr-ft²-°F
     
    Descriptive Properties
    Purity, %99.9995
    Thermal Shock Parameter157°C

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Ceradyne CeraTrex™ SC-P3 Silicon Carbide
    Ceradyne CeraTrex™ 146-IS Silicon Carbide
    Overview of materials for Styrenic Elastomer (TES)
    CeramTec CD 110 Silicon Carbide, SSiC
    Silicon Carbide, sublimed

    CCERDN06 / 689

    New MatWeb Services

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.