MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec CD 110 Silicon Carbide, SSiC
Categories: Ceramic; Carbide

Material Notes: Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applications. SSiC is resistant to all chemical media. Since no metallic silicon is present in the matrix, it can be used at temperatures up to 1600°C without impaired strength.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.10 g/cc0.112 lb/in³DIN EN 623-2
Water Absorption 0.00 %0.00 %Open Porosity; DIN EN 623-2
Permeability 0.000.00%, Gas
Weibull Modulus 1212DINV ENV 843-5
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 25002500HV1; DINV ENV 843-4
Tensile Modulus 415 GPa60200 ksiYoung's; DINV ENV 843-2
Flexural Strength 440 MPa63800 psiDIN EN 843-1
Compressive Strength 2000 MPa290000 psiDIN 51067T1
Poissons Ratio 0.160.16DINV ENV 843-2
Fracture Toughness 3.80 MPa-m½3.46 ksi-in½KIC (SEVNB); DIN CEN/TS 14425-1
Shear Modulus 179 GPa26000 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  10 ohm-cm
@Temperature 400 °C
10 ohm-cm
@Temperature 752 °F
IEC 672-1
 5.00e+7 ohm-cm
@Temperature 20.0 °C
5.00e+7 ohm-cm
@Temperature 68.0 °F
IEC 672-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear  3.50 µm/m-°C
@Temperature 20.0 - 400 °C
1.94 µin/in-°F
@Temperature 68.0 - 752 °F
DIN EN 821-1
 4.30 µm/m-°C
@Temperature 20.0 - 1000 °C
2.39 µin/in-°F
@Temperature 68.0 - 1830 °F
DIN EN 821-1
Specific Heat Capacity 0.600 J/g-°C0.143 BTU/lb-°FDINV ENV 821-3
Thermal Conductivity 100 W/m-K694 BTU-in/hr-ft²-°FDIN EN 821-2
Maximum Service Temperature, Air 1400 °C2550 °F
Maximum Service Temperature, Inert 1800 °C3270 °F
 
Descriptive Properties
Ra = Arithmetic Mean Roughness Value (µm)<0.1
Thermal Shock Resistance R1 (K)240calculated; R1 = [σs (1-µ)] / (α·E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics CVD Silicon Carbide
CoorsTek UltraSiC™ SC-30 Direct Sintered Silicon Carbide
CeramTec Rocar® ST Silicon Carbide, SSiC
Silicon Carbide, Alpha SiC
CeramTec Rocar® S Silicon Carbide, SSiC

CCERA913 / 107513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.