MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow VORANOL™ RA 800 Polyol
Categories: Polymer; Thermoset

Material Notes: VORANOL™ RA 800 polyol is a highly reactive amine initiated polyether polyol, specially developed for the production of rigid polyurethane foams and designed for blending with other polyols.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Viscosity Measure 3550 cSt
@Temperature 37.8 °C
ASTM D445-94
 15000 - 19000 cSt
@Temperature 25.0 °C
ASTM D445-94
Maximum Moisture Content 0.10wt% water; ASTM E203-96
 
Thermal PropertiesOriginal ValueComments
Flash Point 205 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 5.0ASTM D4890-93
 
Descriptive Properties
Basicity meq/g, min3.4 - 3.7DOWM 101485-TE94A
Hydroxyl Number mg KOH/g780 - 820ASTM D4274-94d

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow VORANOL™ 4701 Polyether Polyol
Dow UCON™ 50-HB-260 PAG Lubricant
Dow VORANOL™ 4815 Polyether Polyol
Dow SPECFLEX™ NC 700 Polyol
Dow VORANOL™ 4240 Polyether Polyol

PDOW1482 / 30700

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.