System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Dow VORANOL™ 4701 Polyether Polyol
Categories:
Polymer
;
Thermoset
Material Notes:
VORANOL™ 4701 polyether polyol is a high reactivity capped triol. Its high molecular weight and high primary hydroxyl content make it well suited for high resiliency, flexible molded foams.
Information provided by Dow
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.018
g/cc
1.018
g/cc
Maximum Moisture Content
0.050
0.050
wt% water
ASTM Color
<= 35
<= 35
APHA
Thermal Properties
Metric
English
Comments
Specific Heat Capacity
2.08
J/g-°C
@Temperature 20.0 °C
0.497
BTU/lb-°F
@Temperature 68.0 °F
2.27
J/g-°C
@Temperature 60.0 °C
0.543
BTU/lb-°F
@Temperature 140 °F
2.46
J/g-°C
@Temperature 100 °C
0.588
BTU/lb-°F
@Temperature 212 °F
Thermal Conductivity
0.151
W/m-K
1.04
BTU-in/hr-ft²-°F
0.123
W/m-K
@Temperature 100 °C
0.852
BTU-in/hr-ft²-°F
@Temperature 212 °F
0.126
W/m-K
@Temperature 40.0 °C
0.875
BTU-in/hr-ft²-°F
@Temperature 104 °F
Flash Point
185
°C
365
°F
Descriptive Properties
Hydroxyl Number mg KOH/g
34
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Dow VORANOL™ 4701C Polyether Polyol
Dow VORANOL™ 4703 Polyether Polyol
Dow VORANOL™ 4240 Polyether Polyol
Dow VORANATE™ T-80 toluene diisocyanate (TDI)
Dow VORANOL™ 4815 Polyether Polyol
PDOW1471 / 30689
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.