MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Versalis Impressio® HIPS E05 3D Printing Filament Grade High Impact Polystyrene
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Impressio® HIPS E05 is an easily process able high impact polystyrene with good mechanical and thermal properties. Impressio® HIPS E05 has been optimized for the production of filaments dedicated to 3D printing (FDM).

Applications: Impressio® HIPS E05 has been designed to produce 1.75 and 2.85mm filaments used into 3D printers for the production of prototypes. It can also be used as limonene soluble support phase.

Information provided by Versalis.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ISO 60
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption <= 0.10 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.10 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 6565ISO 2039/2
Tensile Strength at Break 28.0 MPa4060 psi50 mm/min; ISO 527
Tensile Strength, Yield 22.0 MPa3190 psi50 mm/min; ISO 527
Elongation at Break 70 %70 %50 mm/min; ISO 527
Tensile Modulus 1.90 GPa276 ksi1 mm/min; ISO 527
Flexural Strength 38.0 MPa5510 psi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  6.50 kJ/m²
@Thickness 4.00 mm,
Temperature -30.0 °C
3.09 ft-lb/in²
@Thickness 0.157 in,
Temperature -22.0 °F
ISO 180/1A
 10.0 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
4.76 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D 696
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FISO 8302
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °F120°C/h, annealed; ISO 75-2/A
Vicat Softening Point  91.0 °C
@Load 5.10 kg
196 °F
@Load 11.2 lb
50°C/h; ISO 306
 99.0 °C
@Load 1.02 kg
210 °F
@Load 2.25 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Glow Wire Test 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
IEC 60695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 240 °C410 - 464 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9886 / 265639

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.