MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Versalis Impressio® HIPS E05 3D Printing Filament Grade High Impact Polystyrene
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Impressio® HIPS E05 is an easily process able high impact polystyrene with good mechanical and thermal properties. Impressio® HIPS E05 has been optimized for the production of filaments dedicated to 3D printing (FDM).

Applications: Impressio® HIPS E05 has been designed to produce 1.75 and 2.85mm filaments used into 3D printers for the production of prototypes. It can also be used as limonene soluble support phase.

Information provided by Versalis.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.650 g/ccISO 60
Density 1.04 g/ccISO 1183
Water Absorption <= 0.10 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 65ISO 2039/2
Tensile Strength at Break 28.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 22.0 MPa50 mm/min; ISO 527
Elongation at Break 70 %50 mm/min; ISO 527
Tensile Modulus 1900 MPa1 mm/min; ISO 527
Flexural Strength 38.0 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²
@Thickness 4.00 mm,
Temperature -30.0 °C
ISO 180/1A
 10.0 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CASTM D 696
Thermal Conductivity 0.170 W/m-KISO 8302
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C120°C/h, annealed; ISO 75-2/A
Vicat Softening Point 91.0 °C
@Load 5.10 kg
50°C/h; ISO 306
 99.0 °C
@Load 1.02 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
Glow Wire Test 650 °C
@Thickness 1.60 mm
IEC 60695-2-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 210 - 240 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENF9886 / 265639

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.