MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Armacell OleTex® CKJN 1000 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes:

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.0 lb/ft³ASTM D3575W
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 224 psiASTM D3575T
Elongation at Break 200 %ASTM D3575T
Compressive Strength 31.0 psi
@Strain 10 %
ASTM D3575D
 45.0 psi
@Strain 25 %
ASTM D3575D
 61.0 psi
@Strain 40 %
ASTM D3575D
 80.0 psi
@Strain 50 %
ASTM D3575D
Tear Strength 71.0 pliASTM D3575G
Compression Set 10 %ASTM D3575B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °F
Minimum Service Temperature, Air -65.0 °F
 
Descriptive Properties
FlammabilityFMVSS302Pass
Thermal Stability<0.5%24 hrs @ 158°F, ASTM D3575S
Water Absorption<0.07 lb/sq ft(skived), ASTM D3575L

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Homopolymer HP0339C20L1 Calcium Reinforced
Bamberger Polymers Bapolene® 1072 Polyethylene, Injection Grade
Bamberger Polymers Bapolene® 4062 Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 4082 Polypropylene, Injection Grade
Braskem H502-25RG Extrusion Polypropylene

PARMD131 / 186742

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.