MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cray Valley Wingtack® 102 Aliphatic C-5 Hydrocarbon Resin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Wingtack® 102 is a higher softening point aliphatic resin with a lower molecular weight distribution than typical C5 resins resulting in excellent compatibility in less polar elastomers and well balanced performance. This light colored resin has exceptionally low odor and volatility.

Product Highlights / Performance Properties:

  • Designed to be compatible with less polar polymers, elastomers, e.g. Natural Rubber, Polyisoprene, SIS, and low VA EVA polymers
Suggested Applications:
  • Hot melt adhesives (HMA)
  • Pressure sensitive adhesives (PSA)
  • Rubber processing
  • Caulks
  • Plastics
  • Window sealants

Information provided by Cray Valley

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D891
Molecular Weight 1000 g/molMn
 2000 g/molMw
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 52.0 °Cmidpoint
Ring & Ball Softening Point 102.5 °CE-950
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 3.0in 50% toluene; E-803
 
Descriptive Properties
AppearanceLight yellow
Clarity0.95E-803a

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCRAYV036 / 316189

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.