Description: Wingtack® 102 is a higher softening point aliphatic resin with a lower molecular weight distribution than typical C5 resins resulting in excellent compatibility in less polar elastomers and well balanced performance. This light colored resin has exceptionally low odor and volatility. Product Highlights / Performance Properties: - Designed to be compatible with less polar polymers, elastomers, e.g. Natural Rubber, Polyisoprene, SIS, and low VA EVA polymers
Suggested Applications: - Hot melt adhesives (HMA)
- Pressure sensitive adhesives (PSA)
- Rubber processing
- Caulks
- Plastics
- Window sealants
Information provided by Cray Valley |