Polybutene-1 (PB-1) grade Toppyl PB 8310M is a random copolymer of butene-1 with high ethylene content. This product is primarily used to modify sealing properties or mechanical properties of other polyolefins such as polypropylene or polyethylene. Toppyl PB 8310M is highly compatible with polypropylene due its similar molecular structure. It is less compatible in blends with polyethylene but it is still easily dispersible. This grade is not intended for medical and pharmaceutical applications. Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America Application: Peelable Film; Specialty Film Market: Flexible Packaging; Rigid Packaging Processing Method: Blown Film; Cast Film Attribute: Good Heat Seal; Good Optical Properties; Good Organoleptic Properties; Good Processability Information provided by LyondellBasell. |