MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Toppyl PB 8310M Polybutene
Categories: Polymer; Thermoplastic; Polybutene

Material Notes: Polybutene-1 (PB-1) grade Toppyl PB 8310M is a random copolymer of butene-1 with high ethylene content. This product is primarily used to modify sealing properties or mechanical properties of other polyolefins such as polypropylene or polyethylene. Toppyl PB 8310M is highly compatible with polypropylene due its similar molecular structure. It is less compatible in blends with polyethylene but it is still easily dispersible. This grade is not intended for medical and pharmaceutical applications.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Peelable Film; Specialty Film

Market: Flexible Packaging; Rigid Packaging

Processing Method: Blown Film; Cast Film

Attribute: Good Heat Seal; Good Optical Properties; Good Organoleptic Properties; Good Processability

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.897 g/ccISO 1183-1
Melt Flow 3.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 10.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25.0 MPaISO 8986-2
Elongation at Break 300 %ISO 8986-2
Flexural Modulus 120 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 81.0 °CTm2; ISO 11357-3
 94.0 °CTm1; ISO 11357-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9842 / 324777

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.