MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil SpectraSyn Ultra™ 1000 High VI Polyalphaolefin (PAO) Fluid  (discontinued **)
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Product Description: SpectraSyn Ultra™ High VI Polyalphaolefin (PAO) have high viscosity indices, low pour points, low traction, good air release, and low foaming tendency. The extremely high viscosity indices translate into improved flow at low temperatures and increased elastohydrodynamic lubricant film thickness at high temperatures. SpectraSyn Ultra™ High VI PAO are frequently combines with other synthetic basestocks (e.g. SpectraSyn Ultra™ PAO, Exterex™ esters, and/or Synesstic™ alkylated naphthalene) to obtain optical viscometric properties. ExxonMobil’s SpectraSyn Ultra™ High VI PAO are particularly suited for applications that require improved wear protection.

Appearance: Bright & Clear

Availability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.855 g/cc
@Temperature 15.6 °C
0.0309 lb/in³
@Temperature 60.1 °F
ASTM D4052
Brookfield Viscosity  170000 cP
@Temperature 32.0 °C
170000 cP
@Temperature 89.6 °F
ASTM D2983
 1.94e+6 cP
@Temperature -4.00 °C
1.94e+6 cP
@Temperature 24.8 °F
ASTM D2983
Viscosity Measurement 307307Index; ASTM D2270
Kinematic Viscosity  340 cSt
@Temperature 140 °C
340 cSt
@Temperature 284 °F
ASTM D445
 100000 cSt
@Temperature 0.000 °C
100000 cSt
@Temperature 32.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 10000 cSt10000 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 1000 cSt1000 cStASTM D445
Evaporation Loss 0.50 %
@Temperature 150 °C,
Time 79200 sec
0.50 %
@Temperature 302 °F,
Time 22.0 hour
ASTM D972
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10[mg KOH/g]; ASTM D974 (mod)
 
Thermal PropertiesMetricEnglishComments
Pour Point -17.8 °C0.000 °FASTM D5950/D97
Flash Point >= 265 °C>= 509 °FCOC; ASTM D92
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4711.471ASTM D1218
 
Descriptive Properties
Color<0.5ASTM D1500
CompositionWater<50 ppm, ASTM D6304 (mod)
Density Correction Factor0.000504 (g/cc)/°CASTM D1250
Kauri-Butanol Value3.2ASTM D1133
Noack Volatility (%)0.3ASTM D5800/DIN 51581

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil SpectraSyn Elite™ 150 Metallocene Polyalphaolefin (mPAO) Fluid
ExxonMobil SpectraSyn Ultra™ 300 High VI Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn Elite™ 300 Metallocene Polyalphaolefin Fluid
ExxonMobil Mobilgear SHC Series 680
ChevronTexaco Cetus® PAO 100

PEX99681 / 175917

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.