MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dover Chemical EM 9400 Air Blown Synthetic, Blown Sperm Oil Replacement
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: EM 9400 is an air-blown synthetic replacement for blown sperm oil. Its properties in regard to emulsion promotion and mineral oil stability are similar to blown sperm oil. EM 9400 is soluble in most mineral oils and organic solvents, but is not soluble in water. EM 9400 improves surface wetting properties of lubricants and preservative oils. Additionally, it offers excellent corrosion protection for ferrous and non-ferrous materials when used in cutting oils and drawing compounds.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc
@Temperature 25.0 °C
0.940 g/cc
@Temperature 77.0 °F
Density 0.935 g/cc0.0338 lb/in³
Saybolt Viscosity at 100°F 400 SUS400 SUS
Saybolt Viscosity at 210°F 70 SUS70 SUS
Kinematic Viscosity at 40°C (104°F) 78 cSt78 cSt
Kinematic Viscosity at 100°C (212°F) 13 cSt13 cSt
ASTM Color 1.51.5
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 2525[mgKOH/g]
 
Thermal PropertiesMetricEnglishComments
Pour Point 12.8 °C55.0 °F
Flash Point >= 177 °C>= 351 °FCOC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER134 / 217753

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.