MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolysis and microbe resistance. It can be extruded and injection-moulded. PEARLTHANE® 16N80 can be used for blown- and cast films, cables, tubing and profiles. When processed by injection moulding, can be used for making technical parts.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 81ASTM D2240
Tensile Strength 5076 psiASTM D412
Elongation at Break 760 %ASTM D412
100% Modulus 0.725 ksi
@Strain 100 %
ASTM D412
300% Modulus 1.16 ksi
@Strain 300 %
ASTM D412
Tear Strength 460 pliASTM D624 (Die C)
Abrasion 20loss (mm³); DIN 53.516
Compression Set 30 %
@Temperature 22.8 °C,
Time 252000 sec
ASTM D395
 42 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 320 - 338 °FMQSA 111
Glass Transition Temp, Tg -53.0 °FDSC, 10ºC/min; DIN 51.007
 
Processing PropertiesOriginal ValueComments
Feed Temperature 355 °F
Nozzle Temperature 380 °F
Zone 1 355 - 380 °F
Zone 2 375 - 410 °F
Zone 3 390 - 430 °F
Zone 4 365 - 390 °F
Die Temperature 365 - 380 °F
Mold Temperature 95.0 °F
Moisture Content <= 0.10 %MQSA 44
Screw Speed 50 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® Clear 15N60D Thermoplastic Polyurethane
Lubrizol Estane® S190A Thermoplastic Polyurethane
Lubrizol Advanced Materials Pearlstick® 45-60/18 Polycaprolactone based TPU
Lubrizol Advanced Materials PEARLCOAT® Activa D126K BL Thermoplastic Polyurethane Elastomer

PMES47 / 88424

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.