PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolysis and microbe resistance. It can be extruded and injection-moulded. PEARLTHANE® 16N80 can be used for blown- and cast films, cables, tubing and profiles. When processed by injection moulding, can be used for making technical parts.All information provided by Merquinsa |