MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Veneering Modules Unifelt 3000XT Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Unifelt Veneering modules, 3000 (HT), 3000 M, XT are made from a blend of high temperature Cerafiber and high alumina fiber. The modules are fabricated into blocks, 12" by 12" (305 mm x 305 mm) using pre-cut Unifelt boards turned edge-grain and glued together.

Applications:

  • Forge furnace
  • Crucible furnace
  • Rotary hearth furnace
  • Holding furnace
  • Heat treating furnace
  • Pusher reheat furnace
  • Ceramic kiln

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.144 g/cc
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.130 W/m-K
@Temperature 260 °C
ASTM C201
 0.150 W/m-K
@Temperature 538 °C
ASTM C201
 0.190 W/m-K
@Temperature 816 °C
ASTM C201
 0.260 W/m-K
@Temperature 1093 °C
ASTM C201
Maximum Service Temperature, Air 1593 °CContinuous Use
 1704 °C
Shrinkage 0.80 %
@Temperature 1316 °C,
Time 86400 sec
 1.2 %
@Temperature 1427 °C,
Time 86400 sec
 1.8 %
@Temperature 1538 °C,
Time 86400 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 87 %after firing
Loss on Ignition(%) 5.0 %after firing
SiO2 13 %after firing
 
Descriptive Properties
Colororange

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool 80 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 3000 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 2600 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber

CMORF70167 / 203465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.