Triton ELL is a premium quality, synthetic, semifluid, extreme pressure (EP) lithium complex grease specially developed for the lubrication of wheel bearings on non-driven truck trailer axles equipped with oil seals. It is formulated to help optimize service intervals and reduce operating costs by providing effective lubrication and cooling of wheel bearings exposed to the prolonged high operating temperatures of over-the-road applications. It also is recommended for use in industrial gearboxes operating at high temperatures where oil leakage is a problem and conventional semifluid greases do not provide adequate service life. Triton ELL is manufactured with a high-viscosity synthetic polyalphaolefin (PAO) base oil and a lithium complex soap thickener. It is fortified with extreme-pressure and antiwear additives plus rust and oxidation inhibitors to provide excellent wear protection, corrosion resistance and long service life. It has outstanding thermal stability at high temperatures and outstanding pumpability at low temperatures for use over a wide range of operating temperatures. Applications: - Wheel bearings on non-driven trailer axles equipped with oil seals
- Plain and rolling-element bearings operating at extreme temperatures
- Conveyors
- Centralized lube systems
- Industrial gearboxes where oil leakage is a problem
Features/Benefits:- Outstanding oxidation resistance and thermal stability at high temperatures
- Outstanding pumpability at very low temperatures
- Excellent wear protection
- Protects against rust and corrosion
- Resists water washout
- Excellent seal compatibility
- Formulated for extended service life
Information provided by Phillips 66 Lubricants. |