MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Triton® ELL NLGI Grade 00
Categories: Fluid; Lubricant; Lithium Gellant; Polyalphaolefin (PAO)

Material Notes: Triton ELL is a premium quality, synthetic, semifluid, extreme pressure (EP) lithium complex grease specially developed for the lubrication of wheel bearings on non-driven truck trailer axles equipped with oil seals. It is formulated to help optimize service intervals and reduce operating costs by providing effective lubrication and cooling of wheel bearings exposed to the prolonged high operating temperatures of over-the-road applications. It also is recommended for use in industrial gearboxes operating at high temperatures where oil leakage is a problem and conventional semifluid greases do not provide adequate service life. Triton ELL is manufactured with a high-viscosity synthetic polyalphaolefin (PAO) base oil and a lithium complex soap thickener. It is fortified with extreme-pressure and antiwear additives plus rust and oxidation inhibitors to provide excellent wear protection, corrosion resistance and long service life. It has outstanding thermal stability at high temperatures and outstanding pumpability at low temperatures for use over a wide range of operating temperatures.

Applications:

  • Wheel bearings on non-driven trailer axles equipped with oil seals
  • Plain and rolling-element bearings operating at extreme temperatures
  • Conveyors
  • Centralized lube systems
  • Industrial gearboxes where oil leakage is a problem
Features/Benefits:
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Outstanding pumpability at very low temperatures
  • Excellent wear protection
  • Protects against rust and corrosion
  • Resists water washout
  • Excellent seal compatibility
  • Formulated for extended service life

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.892 g/cc0.0322 lb/in³
Viscosity Measurement 160160Index
Saybolt Viscosity at 100°F 2400 SUS2400 SUS
Saybolt Viscosity at 210°F 225 SUS225 SUS
Kinematic Viscosity at 40°C (104°F) 420 cSt420 cSt
Kinematic Viscosity at 100°C (212°F) 44 cSt44 cSt
Oxidative Stability 100 hour
@Pressure 0.0207 MPa
100 hour
@Pressure 3.00 psi
Pressure Drop; ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 315 kg695 lb (mass)ASTM D2596
Four Ball Wear <= 0.600 mm<= 0.0236 inScar Diameter; ASTM D2266
Penetration P(60), 1/10 mm 400 - 430400 - 430ASTM D217
Timken Test 24900 g55.0 lbOK Load; ASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
ColorEmerald Green
ThickenerLithium Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Triton® XD5 NGLI Grade 0
Phillips 66 Triton® Grade 100
Eastman Tritan™ MX731 Medical Grade Copolyester

WCON5147 / 198400

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.