MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ineos Nova Styrocell® M742C Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.

Applications: Styrocell M742C is used mainly for producing contour moldings with wall thickness less than 10 mm.

This grade complies with major European and US food contact regulatory regimes, including: European Community Directive 90/128/ECC, including 92/39EEC and 95/EC, relating to plastics materials and articles, intended to come into contact with foodstuffs. Dutch Food Packaging Regulations. Recommendations of German Federal Office of Health (BGA), now regulated by the new Institute of Consumer Health (BGVV), Empfehlung V. US Food and Drug Administration Code of Federal Regulations title 21, sections 177.1640 (Polystyrene) and 178.3010 (Blowing Agents).

Information provided by NOVA Chemicals.

Key Words: Expanded Polystyrene, EPS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.620 g/cc0.0224 lb/in³
Density >= 0.0190 g/cc>= 0.000686 lb/in³Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
 0.0190 - 0.0400 g/cc0.000686 - 0.00145 lb/in³Normal molded density assuming cost optimized selection of processing conditions.
Bead Size 0.400 - 0.700 mm0.0157 - 0.0276 in
 0.360 - 0.850 mm0.0142 - 0.0335 inCarrington Laboratory Analytical Methods 2155
 
Chemical PropertiesMetricEnglishComments
Styrene Content <= 0.10 %<= 0.10 %Residual Styrene Monomer Content per Carrington Laboratory Analytical Methods 3112
Blowing Agent Content >= 5.7 %>= 5.7 %Carrington Laboratory Analytical Methods 3135

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
NOVA Chemicals ARCEL® 730B Expanded Polyethylene/Styrenic Polymer
NOVA Chemicals Expandable Polystyrene (EPS) 33MB Expandable Polystyrene Resin

PNOVA295 / 55193

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.