MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow Continuum™ DGDA-2420 YL2 Bimodal Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Continuum™ DGDA-2420 YL2 Bimodal Polyethylene Resin is produced using Unipol™ II process technology. This product is formulated with UV stabilizers for outdoor storage. This product may be utilized for pipe applications where long-term hydrostatic strength combined with outstanding resistance to slow crack growth and rapid crack propagation is desired. Suitable applications include natural gas distribution pipes.
Industrial Standards Compliance:
    ASTM D 3350: cell classification:
    • Natural – PE277370D
    • Yellow – PE277373E (Note A)
  • NSF International: Standard 14
  • Canadian Standards Association (CSA): B137.4 – PE2708 PLUS
  • Plastics Pipe Institute (PPI):
    • ASTM PE 2708 pipe grade – 1250 psi HDB at 73°F, 800 psi HDS at 73°F, and 1000 psi HDB at 140°F
NOTES: (A) The first 5 numbers of the cell classification are based on natural resin. The last number and letter are based on yellow resin. (natural resin plus 2.0% DFDA 0022 YL2)

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: No; Processing Aid: Yes; Slip: No

Agency Ratings: ASTM PE2708; ISO PE 100

Form: Pellets

Processing Method: Profile Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³Base Resin; ASTM D1505
 0.941 g/cc0.0340 lb/in³Yellow; ASTM D1505
Melt Flow  >= 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
>= 0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 9.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
9.5 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 1.79 MPa>= 260 psiASTM D638
Elongation at Break >= 600 %>= 600 %ASTM D638
Flexural Modulus >= 0.621 GPa>= 90.0 ksi2% Break; ASTM D790B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746A
 
Descriptive Properties
Resistance to Rapid Crack Propagation<28°FTc - S-4 @ 5 bar
 >145 psiPc, S-4: 32°F
 >3000 hrNotched Pipe Test: 176°F
 >560 psiPc, Calculated, Full Scale: 32°F
 15000 hrPENT
Thermal Stability>428°FASTM D3350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF410 / 311103

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.