MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celcon® GC25T POM, 25% Glass Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: Celcon« GC25T is a 25% glass fiber coupled acetal copolymer grade. It offers higher strength than the standard Celcon GC25-A. Celcon GC25T is FDA approved. Celcon GC25T is also exceptionally resistant to fuel. It offers excellent resistance to transportation fuels especially oxygenated fuels.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 g/ccASTM D792
Density 1.57 g/ccISO 1183
Moisture Absorption 0.200 %23°C/50%RH; ISO 62
Water Absorption at Saturation 0.80 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cmISO 294-4
 0.0040 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4
 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 129 MPa5mm/min; ISO 527-2/1A
 20000 psiASTM D638
Elongation at Break 3.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 8630 MPa50mm/min; ISO 527-2/1A
Flexural Strength 202 MPaISO 178
Flexural Modulus 8520 MPaISO 178
 1.20e+6 psiASTM D790
Izod Impact, Notched 1.80 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²ISO 180/1A
Charpy Impact Unnotched 50.0 kJ/m²ISO 179/1eU
 55.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.70 kJ/m²ISO 179/1eA
 7.20 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 27.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 125 µm/m-°CISO 11359-2
Melting Point 165 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 161 °CISO 75-1, -2
 325 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 90.0 - 120 °Ccavity
 190 - 210 °Chot runner
Zone 1 170 - 180 °C
Zone 2 180 - 190 °C
Zone 3 180 - 190 °C
Zone 4 190 - 200 °C
Die Temperature 190 - 200 °C
Melt Temperature 180 - 200 °C
Drying Temperature 80.0 - 100 °C
Dry Time 3.00 hour
Injection Pressure 90.0 - 140 MPa
Hold Pressure 90.0 - 140 MPa
Back Pressure <= 2.00 MPa
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Injection moldingYes
Injection speedslow
PelletsYes
Processing conditions acc. ISO9988-2
Profile extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsamid® AZM 30 BLACK T6LD PA12-GF30
Celanese Celcon® GB25 POM, 25% Glass Reinforced
Celanese Celcon® CF802 POM, Specialty
Delrin Delrin® 577 BK000 POM-GF20
Celanese Celcon® GC25A POM, 25% Glass Reinforced

PHCQ104 / 178559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.