System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Celcon® CF802 POM, Specialty
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
Material Notes:
Celcon« acetal copolymer grade CF802 is a conductive, fuel compatible general purpose acetal copolymer. Celcon« CF802 has been developed to dissipate static electricity from fuel handling systems.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.47
g/cc
0.0531
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.017
cm/cm
0.017
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.016
cm/cm
0.016
in/in
ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
62.0
MPa
8990
psi
50mm/min; ISO 527-2/1A
Elongation at Yield
10 %
10 %
50mm/min; ISO 527-2/1A
Tensile Modulus
3.00
GPa
435
ksi
50mm/min; ISO 527-2/1A
Flexural Modulus
3.10
GPa
450
ksi
ISO 178
Izod Impact, Notched (ISO)
4.80
kJ/m²
2.28
ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched
7.00
J/cm²
33.3
ft-lb/in²
ISO 179/1eU
7.00
J/cm²
@Temperature -30.0 °C
33.3
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched
0.400
J/cm²
1.90
ft-lb/in²
ISO 179/1eA
0.400
J/cm²
@Temperature -30.0 °C
1.90
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour
2130
MPa
309000
psi
ISO 899-1
Tensile Creep Modulus, 1000 hours
1050
MPa
152000
psi
ISO 899-1
Electrical Properties
Metric
English
Comments
Volume Resistivity
300
ohm-cm
300
ohm-cm
IEC 60093
1000
ohm-cm
1000
ohm-cm
ASTM D257
Surface Resistance
2000
ohm
2000
ohm
IEC 60093
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
100
µm/m-°C
55.6
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
120
µm/m-°C
66.7
µin/in-°F
ISO 11359-2
Melting Point
167
°C
333
°F
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi)
100
°C
212
°F
ISO 75-1, -2
Processing Properties
Metric
English
Comments
Processing Temperature
80.0
-
120
°C
176
-
248
°F
cavity
190
-
200
°C
374
-
392
°F
hot runner
Zone 1
170
-
180
°C
338
-
356
°F
Zone 2
175
-
185
°C
347
-
365
°F
Zone 3
180
-
190
°C
356
-
374
°F
Zone 4
185
-
195
°C
365
-
383
°F
Die Temperature
190
-
200
°C
374
-
392
°F
Melt Temperature
180
-
200
°C
356
-
392
°F
Drying Temperature
80.0
-
100
°C
176
-
212
°F
Dry Time
3.00
hour
3.00
hour
Injection Pressure
60.0
-
120
MPa
8700
-
17400
psi
Hold Pressure
60.0
-
120
MPa
8700
-
17400
psi
Back Pressure
<=
2.00
MPa
<=
290
psi
Descriptive Properties
Injection molding
Yes
Injection speed
slow
Pellets
Yes
Processing conditions acc. ISO
9988-2
Screw Speed
slow
slow
slow
slow
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Celcon® GC25T POM, 25% Glass Reinforced
Celanese Celcon® EC90PLUS Acetal Copolymer
Celanese Celcon® GB25 POM, 25% Glass Reinforced
Celanese Celcon® GB10 POM, 10% Glass Reinforced
Envalior Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry)
PHCQ097 / 178552
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.