MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy 45 is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It has a wide acceptance by industrial users, as well as being included in Federal military specifications on brazing filler metals or alloys. It has a narrow melting range which is not apparent in most brazing operations, making it flow freely though a capillary. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys with close joint clearances.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Key Words: AWS BAg-1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 9.34 g/cc
Density 0.340 lb/in³
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000606 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1125 - 1145 °F
Solidus 1125 °F
Liquidus 1145 °F
Maximum Service Temperature, Air 400 °Fcontinuous
 600 °Fintermittent
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1145 - 1400 °FBrazing Temperature
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd 23 - 25 %
Copper, Cu 14 - 16 %
Other, total <= 0.15 %
Silver, Ag 44 - 46 %
Zinc, Zn 14 - 18 %
 
Descriptive Properties
ColorLight Yellow
Electrical Conductivity (% IACS)27.6

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy
Materion Silseal® 700 Silver-Copper Brazing Alloy
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy
Lucas-Milhaupt Silvaloy® 402 Brazing Alloy
Lucas-Milhaupt Silvacote® A50N Brazing Alloy

NBRW030 / 79806

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.