MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt Silvacote® A50N Brazing Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvacote A50N is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel to the silver-copper zinc alloy imparts corrosion properties which retards joint or interface corrosion of the brazed assembly. The nickel element in Silvacote A50N also improves the bond strength when joining the tungsten carbide cutting tips. Typical applications are the joining of 300 series stainless steels in the food, medical, and dental fields.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.98 g/cc8.98 g/cc
Density 8.98 g/cc0.324 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00001175 ohm-cm0.00001175 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 660 - 707.2 °C1220 - 1305 °F
Solidus 660 °C1220 °F
Liquidus 707.2 °C1305 °F
Maximum Service Temperature, Air 371 °C700 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 710 - 843 °C1310 - 1550 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 17.3 - 19.3 %17.3 - 19.3 %
Nickel, Ni 1.53 - 2.33 %1.53 - 2.33 %
Other, total <= 0.137 %<= 0.137 %
Silver, Ag 44.75 - 46.75 %44.75 - 46.75 %
Zinc, Zn 24.62 - 26.62 %24.62 - 26.62 %
 
Descriptive Properties
ColorBrown
Electrical Conductivity (% IACS)15
Flux7.5-10%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy
Overview of materials for AISI 4000 Series Steel
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy

NBRW038 / 79814

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.