Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package. Information provided by Bayer. As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
PC + ABS; Poly(Acrylonitrile-Butadiene-Styrene) |