MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® ET3036 FR PC/ABS Blend  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: (PC+ABS)-Blend; flame retardant; Vicat/B 120 temperature = 122 °C; extrusion grade; UL 94 V-0 (1.5 mm) and V-1 (0.75 mm) (Bayer internal test); for pipe- and corrugated pipe extrusion

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 410000 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
410000 cP
@Shear Rate 1000 1/s,
Temperature 500 °F
melt viscosity; b.o. ISO 11443-A
Melt Flow 22 g/10 min
@Load 5.00 kg,
Temperature 260 °C
22 g/10 min
@Load 11.0 lb,
Temperature 500 °F
cm3/10 min volumetric; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.50 GPa363 ksi1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FISO 75-1,-2
Vicat Softening Point  120 °C
@Load 5.10 kg
248 °F
@Load 11.2 lb
50°C/h; ISO 306
 122 °C
@Load 5.10 kg
252 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  V-1
@Thickness 0.750 mm
V-1
@Thickness 0.0295 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection molding; ISO 294
Injection Velocity 240 mm/sec9.45 in/secISO 294

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® FR3000 PC/ABS Blend
INEOS Styrolution Terluran® GP-22 ABS
INEOS Styrolution Terluran® GP-25 ABS
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced

PB09663 / 150795

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.