MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® LX9013 Plasticized Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Description: VESTAMID LX9013 is a plasticized polyamide 12 compound with an especially high long-term resistance under thermal load. Parts made of this material absorb only little moisture, thus leading to nearly unaffected dimensions and properties at changing ambient conditions. VESTAMID LX9013 is suited to produce flexible tubes that are impact-resistant also at low temperatures. These tubes are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles, particularly as fuel lines in diesel engine vehicles. The advantages of the compound to comparable standard grades are strongly obvious in storage tests with diesel fuel.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 43.0 MPaISO 527
Tensile Stress at Strain 30.0 MPa
@Strain 50 %
ISO 527
Elongation at Break >= 150 %ISO 527
Tensile Modulus 0.400 GPa1 mm/min; ISO 527
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 14.0 J/cm²
@Temperature 23.0 °C
Partial Break; ISO 179/1eA
Impact NB8x1 mm tube as molded at -40°C; SAE J2260, SAE J844, ISO 7628-2/DIN 73378
 NB
@Temperature -40.0 °C
8x1 mm tube after 2 h in boiling water; SAE J844
 NB
@Temperature -40.0 °C
8x1 mm tube after 24 h/110°C; SAE J844
Impact Test NB8x1 mm tube as molded 72 h/150°C; ISO 7628-2/DIN 73378
 
Thermal PropertiesOriginal ValueComments
Melting Point 172 °C2. heating; ISO 3146
 
Descriptive Properties
Burst Test Hoop Stress24.8 MPA8x1 mm tube, DIN 53758

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® L2123 Plasticized Nylon 12
Evonik Vestamid® L2140 sw 9.7504 (as-conditioned) Nylon 12
Evonik Vestamid® L2140 sw 9.7504 (dry properties) Nylon 12
Evonik Vestamid® X7393 Plasticized Nylon 12
Evonik Vestamid® X7393 sw (dry properties) Nylon 12

PHULA56 / 47416

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.